1. SEA CEMENT FOR EXPORT
Sea cement used for construction on the sea as jetty, airport on the island and structures, embankments...
Viet nam standard TCVN 606: 2004(American standard ASTM C150-05 & England BS 4027: 1996)
No |
Name of target |
Unit |
Follow TCVN 6067:2004 |
Follow ASTM C 150-05 |
Fllow BS 4027:1996 | ||
PCSR30 |
PCSR40 |
Type V |
32.5N |
42.5N | |||
1 |
Compressive strength limited After 2 days After 3 days After 7 days After 28 days |
N/mm2 |
- ≥ 12 - ≥ 30 |
- ≥ 16 - ≥ 40 |
- ≥ 8 ≥ 15 ≥ 21 |
- - ≥ 16 ≥ 32.5 |
≥ 10 - - ≥ 42.5 |
2 |
Finely ground - Rest on the sieve 0,08 mm - Surface determined by the method Blaine |
% Cm2/g |
≤ 12 ≥ 2800 |
≤ 10 ≥ 3000 |
≥ 2800 |
||
3 |
Time of agglomerated - Start - Finish |
Minutes |
≥ 45 ≤ 375 |
≥ 45 ≤ 375 |
≥ 60 | ||
4 |
volume stability by Le Chatelier |
Mm |
≤ 10 |
≤ 10 | |||
5 |
MKN |
% |
≤ 3 |
≤ 3 |
≤ 3 | ||
6 |
MgO |
% |
≤ 5 |
≤ 6 |
- | ||
7 |
SO3 |
% |
≤ 2.5 |
≤ 2.3 |
≤ 2.5 | ||
8 |
C3A |
% |
≤ 3.5 |
≤ 5 |
≤ 3.5 | ||
9 |
C4AF+2C3A |
% |
≤ 25 |
≤ 25 |
- | ||
10 |
Residue Insoluble |
% |
≤ 1 |
≤ 0.75 |
≤ 1.5 | ||
11 |
Swelling sulfate in 14 days |
% |
≤ 0.04 |
≤ 0.04A |
- | ||
12 |
Na2O+0,658K2O |
% |
0.6 |
0.6A |
0.6 | ||
13 |
Clo |
% |
- |
- |
≤ 0.1 |
2. STONE FOR EXPORT
Size of stone 10 x 28mm (or many size: 1 x 2 - 10x25mm, 10x22mm or stone 1x2 (stone 1x1), 10x16mm, .... Products for pouring concrete as buildings, airport runways, wharf, highways, particularly widely used in factories fresh concrete or hot asphalt…
Hole sieve size (mm) |
Volume of rest on sieve, % volume, size of min and max | ||
Kind of stone : 5 ÷ 10 |
Kind of stone : 10 ÷ 20 |
Kind of stone 20 ÷ 40 | |
5 |
≥ 90 |
- |
- |
10 |
≤ 5 |
≥ 90 |
- |
20 |
- |
≤ 5 |
≥ 90 |
40 |
- |
- |
≤ 5 |